The following formulation requires the use of a colloid mill to produce stable emulsion Water/88.50 ARMAK 1714/0.25 Paraffin wax/10.00 ARMAK 1574 Acetic acid/0.25 ARMAK 1959/1.00
配制方法:
The Armak chemicals and paraffin are heated until clear, 140'F. The melt is added in a thin stream to the water-acetic acid mixture also heated to 140'F using good agitation.