配方类型:
POLISHES, ABRASIVES
配方说明:
Buffing & Polishing Media (Medium-High Pressure Color or Bright
finish)
配方组成:
Triethanolamine -85%/0.50 TO 1.50 Loading Levels %
TRIPOLI R-15/40.0 to 45.0 Loading Levels %
Stearic Acid (B Flakes)/5.0 TO 6.5 Loading Levels %
TRITON X-100/0.0025 TO 0.0050 Loading Levels %
Water/45.0 TO 55.0 Loading Levels %
TRIPOLI C-15/COMBINED Loading Levels %
Pale Oil/0.025 TO 0.050 Loading Levels %
配制方法:
Mix Stearic Acid and Pale Oil in mixer. Add 100 gallons of hot water. Heat to 160'F. Start mixer and begin adding half of the Tripoli R-15. Blend in the Triton X-100 and the balance of the hot water (approximately 60% of total water). Add balance of the Tripoli R-15 and the Tripoli C-15. Let mix until it appears smooth. If temperature is at 160'F and mixture is smooth, mix the Triethanolamine while turning the heat off the mixer. Add a little hot water to help the Triethanolamine mix well. Add the balance of (cold) water to the mixture. Cool mix to 130'F. Pull mixture into drums and let cool.
NOTE: Add 5% Dowacide in hot weather to keep down bacteria.