The Polargel and CMC are dry blended and then slowly added to the water while agitating with the maximum available shear. The B ingredients are added individually to the dispersion and thoroughly mixed until uniform. Preservatives and perfumes may be added at the desired levels after the complete addition of B. Polargel T may be replaced with Hectabrite AW in this formulation at 1.5 to 1.75% with the difference being made up by increasing the amount of water.