Dry Mix Polargel T and Xanthan Gum together. Sift into water and Hyprochlorite mixture. Add calcium carbonate and sodium tripolyphosphate with high shear mixing. Reduce mixing speed and add Dowfax. Polargel T may be replaced with Hectabrite AW or Hectabrite DP in this formulation at 1.5 to 1.7% with the difference being made up by increasing the amount of water.