Slowly add Magnabrite S to water under continuous mixing. Allow the Magnabrite S to hydrate under the maximum available shear for a minimum of 30 minutes. Add the propylene glycol and heat to 75'C. Slowly add Vinol 523, stir and cool. Dissolve the Trycol OAL in Ethanol with moderate heating. Slowly add Phase B to Phase A under continuous mixing and allow to cool.