Dry blend Magnabrite HV and Cellulose Gum and slowly add to the water while agitating at maximum available shear. Add Methyl Paraben and heat with rapid agitation to 85'C. Slowly add pigments from Phase A to Magnabrite/CMC dispersion. Recirculate through a colloid mill or homogenizer-tight gap and retare for water loss. Mix Phase B into Phase A. Follow immediately with Phase C. Cool to 35'C.