Combine (1), (3), and (5) into half of the mineral spirits (4). Heat with agitation to 90'C until wax melts and a clear solution results. Add (7) morpholine to neutralize wax and add (2) Silicone and remainder of mineral spirits (4) while agitating at 90'C. Slurry Kaopolite-1152 into the water with high agitation. Add hot solution (C) to the Slurry (D) and remove heat while continuing to mix until paste polish reaches 55'C. Pour into containers.