In main vessel, melt Phase B materials at 70'C. In side vessel dissolve the polyacrylamide t 75'C. Add Carbopol solution to complete Phase A, mix until uniform. Add Phase A to Phase b with rapid agitation. Cool to 50'C with sweep agitation. Add Phase C and mix until uniform. Combine Phase D, add to batch. Cool to room temperature, add Phase E.