Blend VEEGUM and CMC. Slowly add to the water, while agitating at maximum available shear. Continue mixing until smooth. Micropulverize C. Add to B and grind to a smooth paste. Add to A and heat to 65'C. Heat D to 70'C and add to A/B/C/. Mix until cool.