Disperse the Polymer JR with good agitation thoroughly in the water. Add remaining ingredients of Part A. Mix slowly while heating to 75 C. Continue mixing and cool to 40 C. Add Part B. Continue mixing and cool to 35 C. Add citric acid to pH adjustment of 6.5. Filter. Pack.