Add the Tetronic polyols to water, mixing slowly until dissolved. Mix in propylene glycol, Marcol 70, and Lanogene. Add Snow White and Polawax A31 and heat gently until solids melt. Homogenize briefly, add perfume and preservative and transfer to suitable containers. Note: Product is a viscous cream at room temperature.