Combine propylene glycol and Promyristyl PM3. Dust in sodium stearate with good agitation, avoiding lumping. When uniformly dispersed, add Irgasan DP300, and heat to 80-85 C. Slowly add water. System should become crystal clear, with skinning occurring on the surface. Add fragrance and Fill into molds. Note: If cloudiness occurs due to the fragrance, or loss of water, clarity can easily be restored by adding up to 10% more propylene glycol.