Add the solvents, except dimethylformamide, to BKS-2750 solution. Dissolve the dicyandiamide in the dimethylformamide and add this solution to the diluted BKS-2750 solution. Physical Properties: Solids---26.28% Sp. Gr.---0.960 Wt./Gal---8.01 lb Visc. (Gardner)---As Note: Apply by spray, dip, or roller coat. Maximum performance is obtained at a 0.3-0.7 mil film thickness. Bake for 5-10 min at 400 F (204 C) or follow an equivalent schedule.