Prepare Part A and Part B separately with good agitation at room temperature until clear and uniform. If necessary, heat Part B after initial dispersing of Quatrisoft^T^M Polymer LM-200. Cool to room temperature. Add Part B to Part C. ADd Part D to Part A, avoiding air entrapment. Add Parts B/C to A/D and mix until clear and uniform.