Disperse Polymer JR in water by heating to about 50 C with moderate agitation. Add citric acid, Dowicil 200, and propylene glycol with continued agitation to obtain a uniform mixture. Heat to 65 C and add ethylene glycol distearate with continued agitation to obtain a uniform mixture. Discontinue heating. Add Sipon L-22, Sipoteric COB, and Sipoteric 1442 singly with sufficient agitation to obtain a uniform mixture before making next addition. At 45-50 C add a suitable fragrance and color. Physical Properties: Appearance---white opaque liquid Visc. (@ 25 C)---10,700 cps pH---5.5 Solids---23.65%