Weigh Part A ingredients into a mixing vessel and mix for 10 min. Having made the water alkaline, Methocel polymers (Part B) can be slowly sprinkled in and will dissolve with mixing after about 15 min. Combine and dissolve Part C ingredients. When dissolved, add to Part A batch and mix for 10 min. Add color (Part D) and mix for an additional 10 min. Slowly add sodium laureth sulfate (Part E) to the batch and mix for 15 min (or until the batch is homogeneous). Combine Part F ingredients and heat to 40 C. Then mix to solubilize the perfume oil. Add Part F solution to batch and mix for 10 min.