Add Quatrisoft^T^M Polymer LM-200 to the water (water phase, Part A). Mix until thoroughly dispersed, then heat to 45-50 C. Mix until clear and uniform. Add Water Phase Part A to Water Phase Part B with mixing while heating to 70 C. Heat Oil Phase to 70 C. Add Water Phase at 70 C to Oil Phase at 70 C while mixing. Cool to 35 C.