Bitumen (180-210 Pen.)/8 Sand/45 Stone (0.25 in.)/20 Rubber Powder/0.2-0.4 Portland Cement/11 Stone (0.125 in.)/16
配制方法:
The rubber powder is heated with the bitumen in the usual way. The finished thickness of the surface is 0.5 in. and within 0.5 hour of laying, it is ready for use.