"WSP" X-250/3.00 Polymer JR 30-M/1.00 "BARQUAT" CT-29 (30% active sol.)/7.00 Citric acid (anhydrous)/0.03
配制方法:
Add Citric acid to water and heat to 60-65'C. Slowly add "Polymer JR"-30-M with high speed mixing. Temperature need not be retained at 60'C. When "Polymer" JR-30-M has been completely dissolved, cool mixture to room temperature and add WSP X-250 and "BARQUAT" CT-29. Continue mixing until a uniform solution has been achieved.