配方类型:
PAPER
配方说明:
Paper Coating
配方组成:
Glyoxal/0.48
Latex/8.00
Water as needed for a solids content of 555 to 60%
No. 11 Roll Coater (For Letterpress Paper
Preservative/-
*the casein should be cooked for 45 min at 55'C in the presence of 14%
aqueous ammonia (based on dry casein). the casein solution should then
be slowly added to the pigment dispersion.
Clay (predispersed)/100.0
Butadiene-styrene latex/18.0
Dispersant/0.1
"Vinol" 125 polyvinyl alcohol/3.0
"Virset" A-130/0.5
Surfynol PC defoamer/0.1
Lubricant (solids)/1.0
"Aircoflex" 100 (solids)/16.0
LV protein, NH4OH cut/-
Clay (predispersed)/90.0
Titanium dioxide/10.0
Dispersant/0.1
CaCO3, precipitated/35.00
"Vinol" 125 polyvinyl alcohol/5.0
"Virset" A-130/1.0
Enzyme converted starch/-
"Surfynol" PC defoamer/0.1
Lubricant (solids)/1.0
"Aircoflex" 100 (solids)/10.0
T.S.P.P../-
Clay (predispersed)/90.0
Preservative/-
Titanium dioxide/10.0
Dispe
配制方法:
Water as needed for a solids content of 55% to 60%.