High-flash naphtha or kerosene/65.0 Butyl "Cellosolue"/2.0 Oleic acid/5.4 Pine oil/24.0 Triethanolamine/3.6
配制方法:
This formulation is generally used simultaneously with a water phase containing one or several alkaline sodium salts or similar coupler. At room temperature, blend by stirring the pine oil and oleic acid. Then, in order, add the triethanolamine and coupler. Slowly add the petroleum solvent and continue stirring until product appears uniform.