Disperse all "QYNV" in R2H until a uniform paste is formed. Then add the pigment gradually until all is dispersed well. Add G-62 and Mark Ll and finally the solvent. Do not overheat during dispersion. Note that the paint thickens up in about 1 or 2 weeks on standing. Therefore more solvent should be added to bring the paint to the cating viscosity if it is to be used at a later date.