Dissolved the parabens in boiling water. Disperse the methylcellulose with agitation. Allow to cool and gel to form. Add water. Slurry magnesium oxide in gel mixture with agitation. Disperse calcium carbonate with agitation. Add saccharin, peppermint oil, and bring to full volume. Pass through colloid mill and a straining tank.