Disperse all "QYNV" in plasticizer until a uniform paste is formed. Then add the pigment gradually until all is dispersed well. Add G-62 and Mark LL and finally the solvent. Do not overheat during dispersion. Note that the paint thickens up in about one or two weeks on standing. therefore, more solvent should be added to bring the paint to the coating viscosity if it is to be used at a later date.