Lead Dioxide Curing Pastes and Powders for "P" Polysulfide Liquid Polymers
配方组成:
Lead dioxide/50 Recommended Ratio Lead stearate/- Lead stearate/- Aluminum distearate/- Stearic acid/- Dibutyl Phthalate/- Toluene/- "Aroclor" 1254/50 Parts per 100 LP-2/15 Set time at 80'F. and 50% RH/5-15 Mins. Lead dioxide/50 Lead stearate/- Aluminum distearate/10 Stearic acid/- Dibutyl Phthalate/- Toluene/- "Aroclor" 1254/- Parts per 100 LP-2/9 Set time at 80'F. and 50% RH/8-16 hrs. Lead dioxide/50 Lead stearate/8 Aluminum distearate/- Stearic acid/- Dibutyl Phthalate/- Dibutyl Phthalate/- Toluene/- "Aroclor" 1254/- Parts per 100 LP-2/9 Set time at 80'F. and 50% RH/8-16 hrs. Lead dioxide/50 Lead stearate/- Aluminum distearate/- Stearic acid/5 Dibutyl Phthalate/45 Toluene/- Aluminum distearate/- "Aroclor" 1254/- Toluene/38 Lead dioxide/50 Parts per 100 LP-2/15 Set time at 80'F. and 50% RH/3-4 hrs. P