"Heat the "Armowax" and "Armeen" to approximately 140'C. (284'F.). Add in a thin stream to the water and acetic acid heated to approximately 100'C. (212'F.), using vigorous agitation. continue stirring until smooth. For maximum fineness of particle size, use a colloid mill or equivalent.