Nickel-molybdate colors may be produced on spangled, tinned steel by making it cathode in the following solution Ammonium molybdate/50 g/l pH/4-6 Boric acid/30 g/l Temperature/30-60'C Nickel sulfate/100 g/l Time/2-5 minutes Current density/0.4-3 A/dm^2